Update: I quit using coolant on aluminum and my finish got sharper
I know this goes against what most of the shop floor says, but I stopped flooding aluminum parts with coolant about 8 months ago and I am not going back. For years I ran the pump wide open on every 6061 job because that is what the guy who trained me at the shop in Mesa always did, and I just never asked why. What changed was a rush job last fall, 400 small brackets, and the coolant tank was low so I ran them dry with just a little air blast to clear the chips. The finish came out cleaner than any wet run I had done on that machine, no spotting, no gumming up the flutes, and my inserts lasted longer than usual. I started reading up and testing it on scrap, and for light finishing passes the coolant was actually shocking the part and making my numbers drift on the mics. Now I rough with a little mist and finish dry, and I am holding tenths way easier than I did chasing coolant dilution all day. Has anyone else run aluminum dry on finish passes, or am I going to get yelled at by the next guy who takes over my machine?