Unpopular opinion: a horseshoe does NOT count as a heat treat test
Had a guy swing by my shop in Akron with a horseshoe he bought at a flea market, saying it was 'forge welded and fully hardened' so he knew the steel was good. I tossed it in the forge at about 1500 degrees and it slumped into a banana shape in under 3 minutes, which told me nobody ever quenched it right. What's the weirdest thing a customer has brought in claiming it was properly heat treated?
Fully hardened" is doing a lot of work in that sentence, considering the thing folded like warm taffy. A real quench would have it fighting the hammer, not drooping at forge heat. Did the seller give him any story about who made it, or was it just a flea market handshake and a prayer?